I use ACF-50, Boeshield, LPS-3, linseed oil, or paralketone, on aluminum or
steel. The latter two last longer and all 3 flex well.
Some steel takes well to cadmium plating, but you have to send it off to a
reputable electroplater. And cadmium-plating sends the environmentalists
into pavlovian convulsions.
|