Thread: Urethane Paint
View Single Post
  #7  
Old November 15th 15, 01:17 PM posted to rec.aviation.soaring
son_of_flubber
external usenet poster
 
Posts: 1,550
Default Urethane Paint

On Sunday, November 15, 2015 at 4:34:23 AM UTC-5, Paul Crabb wrote:

PU or Acrylic topcoat paint is just used as a very thin UV block, it is usually a very thin layer and is not used to "profile" the surface.


Does the PU protect the gelcoat from temperature related crazing?
Someone told me that gelcoat crazing was attributed to rapid change in temperature associated with flying wave. Once the cracks start moisture penetrates and accelerates the deterioration.

Anyone have a crazed PU painted wing?

Anyone have a better explanation for wing crazing?