[ ]"They were out of the plate but not the tubing [ ] Mike"

Actually they are out of 'normaized' condition 4130 plate/sheet.
In the mean time annealed condition is still avaliable. Would an experienced
member please outline procedure for normalizing from annealed back to usable
normalized condition (prior?) to cutting out parts.