Normalizing was heating the steel to snipped
above the critical point, but letting
it air-cool in still air. This would mean a cooling time of 15 minutes to
45 minutes. In no case was the hot steel dipped in oil or anything else (as
was mentioned in an earlier post). That is quenching, a completely
different process.

snipped
You`r right Harry O. I was thinking of when we would draw tool steel down to a
normalized R "c" reading in the draw furnace and try to avoid hard spots. i.e.
mold steels etc.
Thanks for the correction.

Warren

 




Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT +1. The time now is 07:44 AM.


Powered by vBulletin® Version 3.6.4
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Copyright ©2004-2024 AviationBanter.
The comments are property of their posters.