" jls" wrote:

"Richard Riley" wrote in message
...
I've just finished machining my instrument panel. It is (I say with
no small pride) nice. Milled out of 2024T3 3" thick, reduced to .120
with .120 webs between each instrument and around the perimeter.

Now the question is: how should it be finished? Polished? Engine
turned? Anodized? Clear powder coat?


Alodine it and then put up a frilly little placard that says 24K. It would
be reminiscent of you.



If you first polish it, then dip it in alodyne, it will look like a
piece of gold jewelry.